Resin Technology Group TIGA 216-EX High Performance Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 216-EX High Performance Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mix ratio 2 to 1 by volume.TIGA 216-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 216-EX offers a 60 minute pot life and good hardness development within a few hours of mixing. TIGA 216-EX is a toughened epoxy exhibiting rugged chemical and environmental resistance and durability. TIGA 216-EX is an excellent general purpose adhesive providing exceptional bond strength to a wide variety of substrates, PVC, FRP, Polyacrylic, Steel, and many more.Applications: TIGA 202-EX is excellent for general purpose high speed industrial assembly, electronic applications, component attachment to boards, housing assembly and potting.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Of hardener
1.12 g/cc
1.12 g/cc
Of resin
Viscosity 60000 cP

@Temperature 25.0 °C
60000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D >= 80
>= 80
Cured 12 hours at 25°C
75 - 85
75 - 85
Cured 24 hours at 25°C
80 - 85
80 - 85
Shear Strength >= 27.6 MPa
>= 4000 psi
2 hours, 65°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min
Small Mass(15gr.)
Descriptive Properties Value Comments
Color Off-white/Opaque