| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Cycoloy® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 |
| 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
| 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 85 % | 85 % | 50 mm/min; ISO 527 |
| 110 % | 110 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 4.6 % | 4.6 % | Type I, 50 mm/min; ASTM D638 |
| 5.0 % | 5.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.38 GPa | 345 ksi | 1 mm/min; ISO 527 |
| 2.55 GPa | 370 ksi | 50 mm/min; ASTM D638 | |
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
| 93.0 MPa | 13500 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.48 GPa | 360 ksi | 2 mm/min; ISO 178 |
| 2.49 GPa | 361 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
| 2.02 J/cm @Temperature -30.0 °C |
3.78 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 51.0 kJ/m² | 24.3 ft-lb/in² | 80*10*4; ISO 180/1A |
| 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 5.40 J/cm² | 25.7 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 50.0 J @Temperature -30.0 °C |
36.9 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
| 53.0 J @Temperature -40.0 °C |
39.1 ft-lb @Temperature -40.0 °F |
ASTM D3763 | |
| 56.0 J @Temperature 23.0 °C |
41.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 129 °C | 264 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 107 °C @Thickness 3.20 mm |
225 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |