| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP Lubriloy |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
| 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.300 % | 0.300 % | 50% RH, 24 hrs; ASTM D570 |
| 0.430 % | 0.430 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0257 cm/cm @Time 86400 sec |
0.0257 in/in @Time 24.0 hour |
ISO 294 |
| 0.026 cm/cm @Time 86400 sec |
0.026 in/in @Time 24.0 hour |
ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.026 cm/cm @Time 86400 sec |
0.026 in/in @Time 24.0 hour |
ASTM D955 |
| 0.026 cm/cm @Time 86400 sec |
0.026 in/in @Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 43.0 MPa | 6240 psi | ASTM D638 |
| 43.0 MPa | 6240 psi | ISO 527 | |
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
| 47.0 MPa | 6820 psi | ASTM D638 | |
| Elongation at Break | 29.6 % | 29.6 % | ISO 527 |
| 38.6 % | 38.6 % | ASTM D638 | |
| Elongation at Yield | 6.0 % | 6.0 % | ASTM D638 |
| 8.8 % | 8.8 % | ISO 527 | |
| Tensile Modulus | 1.99 GPa | 289 ksi | 50 mm/min; ASTM D638 |
| 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 67.0 MPa | 9720 psi | ASTM D790 |
| 69.0 MPa | 10000 psi | ISO 178 | |
| Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
| 2.20 GPa | 319 ksi | ISO 178 | |
| Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 137 kJ/m² | 65.2 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
| Coefficient of Friction, Dynamic | 0.31 | 0.31 | ASTM D3702 Modified |
| Coefficient of Friction, Static | 0.27 | 0.27 | ASTM D3702 Modified |
| K (wear) Factor | 24.2 x 10<sup>-8</sup> mm³/N-M | 12.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 66.0 °C @Thickness 3.20 mm |
151 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 67.0 °C | 153 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 62.0 °C @Thickness 3.20 mm |
144 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL 94 by SABIC-IP |