| Category | Polymer , Thermoplastic , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP STAT-KON |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP STAT-KON CD0001 PS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
| Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.100 % | 0.100 % | 50% RH, 24 hrs; ASTM D570 |
| 0.130 % | 0.130 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm @Time 86400 sec |
0.0030 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0070 cm/cm @Time 86400 sec |
0.0040 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 16.0 MPa | 2320 psi | Type I, 5 mm/min; ASTM D638 |
| 17.0 MPa | 2470 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | Type I, 5 mm/min; ASTM D638 |
| 23.0 MPa | 3340 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 7.1 % | 7.1 % | 5 mm/min; ISO 527 |
| 9.7 % | 9.7 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 1.2 % | 1.2 % | Type I, 5 mm/min; ASTM D638 |
| 1.2 % | 1.2 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
| 2.28 GPa | 331 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 40.0 MPa | 5800 psi | ISO 178 |
| Flexural Yield Strength | 42.0 MPa | 6090 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
| 2.28 GPa | 331 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.820 J/cm | 1.54 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 7.44 J/cm | 13.9 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 107 µm/m-°C @Temperature -40.0 - 40.0 °C |
59.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 87.0 °C @Thickness 3.20 mm |
189 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 75.0 °C @Thickness 3.20 mm |
167 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 3.0 - 5.0 ohm | 3.0 - 5.0 ohm | ASTM D257 |