Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DD000CEX PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 7.4 %
7.4 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
50 mm/min; ASTM D638
Flexural Strength 96.0 MPa
13900 psi
ASTM D790
Flexural Modulus 2.72 GPa
395 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 137 °C

@Thickness 3.20 mm
279 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 10000 - 1.00e+7 ohm
10000 - 1.00e+7 ohm
ASTM D257