| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
| Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.540 % | 0.540 % | 50% RH, 24 hrs; ASTM D570 |
| 0.810 % | 0.810 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm @Time 86400 sec |
0.0060 - 0.0080 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 26.0 MPa | 3770 psi | 5 mm/min; ISO 527 |
| 27.0 MPa | 3920 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
| 38.0 MPa | 5510 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 29 % | 29 % | 5 mm/min; ISO 527 |
| 31 % | 31 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 4.0 % | 4.0 % | Type I, 5 mm/min; ASTM D638 |
| 4.0 % | 4.0 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 1.55 GPa | 225 ksi | 1 mm/min; ISO 527 |
| 1.66 GPa | 241 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 49.0 MPa | 7110 psi | ISO 178 |
| Flexural Yield Strength | 54.0 MPa | 7830 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 1.49 GPa | 216 ksi | 2 mm/min; ISO 178 |
| 1.63 GPa | 236 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 1.31 J/cm | 2.45 ft-lb/in | ASTM D256 |
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
| Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 33.0 J | 24.3 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
5.56 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| CTE, linear, Transverse to Flow | 109 µm/m-°C @Temperature -30.0 - 30.0 °C |
60.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 77.0 °C | 171 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 66.0 °C @Thickness 3.20 mm |
151 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
| Static Decay | <= 1.0 sec | <= 1.0 sec | 5000V to <50V; FTMS101B |