| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® PK2870 PC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.150 % | 0.150 % | 23°C / 50% RH; ISO 62 |
| Moisture Absorption at Equilibrium | 0.35 % | 0.35 % | ASTM D570 |
| 0.58 % @Temperature 100 °C |
0.58 % @Temperature 212 °F |
ASTM D570 | |
| Water Absorption at Saturation | 0.35 % | 0.35 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 2.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 2.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| 4.0 g/10 min @Load 2.16 kg, Temperature 300 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ISO 2039-2 |
| Tensile Strength at Break | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 |
| 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
| 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | >= 70 % | >= 70 % | Type I, 50 mm/min; ASTM D638 |
| >= 70 % | >= 70 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 7.0 % | 7.0 % | Type I, 50 mm/min; ASTM D638 |
| 7.0 % | 7.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.35 GPa | 341 ksi | 50 mm/min; ASTM D638 |
| 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 93.0 MPa | 13500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
| 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ASTM D4812 | |
| Izod Impact, Notched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*3; ISO 180/1A |
| 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 170 J | 125 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C177 |
| 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 145 °C | 293 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 145 °C @Thickness 3.20 mm |
293 °F @Thickness 0.126 in |
ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 130 °C | 266 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
ASTM D648 | |
| Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ISO 306 |
| 150 °C | 302 °F | Rate B/120; ISO 306 | |
| 150 °C | 302 °F | Rate B/50; ASTM D1525 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.586 | 1.586 | ISO 489 |
| Haze | <= 0.80 % @Thickness 2.54 mm |
<= 0.80 % @Thickness 0.100 in |
ASTM D1003 |
| Transmission, Visible | 88 % | 88 % | 2.54 mm; ASTM D1003 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |