Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC PP681K Polypropylene Random Copolymer for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer SABIC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC PP681K Polypropylene Random Copolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: PP 681K is specially developed for producing injection molded articles with high clarity and also has better impact properties than homo PP counterparts.PP 681K has the following features:Consistent processabilityGood stiffnessExcellent clarityTypical Applications: PP 681K can be used for clear housewares items, lids, food containers, baby bottles (ISBM), caps and CD-boxes.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus, 1% Secant 1050 MPa
152000 psi
ASTM D790A
Izod Impact, Notched 0.650 J/cm
1.22 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM D648
Vicat Softening Point 127 °C
261 °F
ASTM D1525B
Processing Properties Metric English Comments
Processing Temperature 200 - 230 °C
392 - 446 °F
Barrel Temperature
Mold Temperature 15.0 - 40.0 °C
59.0 - 104 °F
Users viewing this material also viewed the following: