Material Notes:
Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0070 - 0.012 cm/cm

@Thickness 3.00 mm
0.0070 - 0.012 in/in

@Thickness 0.118 in
ASTM D955
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 250 °C
18 g/10 min

@Load 8.38 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Yield Strength 63.7 MPa
9250 psi
ASTM D790
Flexural Modulus 1.77 GPa
256 ksi
ASTM D790
Izod Impact, Unnotched 6.86 J/cm

@Thickness 3.17 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
584 kV/in
ASTM D149
Dissipation Factor 0.0090

@Frequency 1.00e+6 Hz
0.0090

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 118 sec
118 sec
ASTM D495
Processing Properties Metric English Comments
Rear Barrel Temperature 230 - 250 °C
446 - 482 °F
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Front Barrel Temperature 210 - 230 °C
410 - 446 °F
Nozzle Temperature 240 - 250 °C
464 - 482 °F
Melt Temperature 240 - 250 °C
464 - 482 °F
Drying Temperature 120 °C
248 °F
Dry Time 3 - 5 hour
3 - 5 hour
Moisture Content <= 0.020 %
<= 0.020 %
Screw Speed 30 - 80 rpm
30 - 80 rpm