Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® FRGF1850-BK1 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® FRGF1850-BK1 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-93
Elongation at Break 2.0 %
2.0 %
ISO 527-93
Flexural Strength 190 MPa
27600 psi
ISO 178-93
Flexural Modulus 8.70 GPa
1260 ksi
ISO 178-93
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
ISO 75-93
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in