| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded |
| Manufacturer | Zhejiang Juner New Materials Co. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Zhejiang Juner JEPP2007 PP For Automotive Parts.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | GB/1033 |
| Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | GB/15585 |
| Melt Flow | 1.0 - 1.3 g/10 min | 1.0 - 1.3 g/10 min |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | GB/1040 |
| Flexural Strength | 30.0 MPa | 4350 psi | GB/9341 |
| Charpy Impact Unnotched | NB | NB | IS0179-1:2000 |
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | IS0179-1:2000 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 115 °C | 239 °F | GB1634 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 170 - 230 °C | 338 - 446 °F | |
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
| Injection Pressure | 30.0 - 90.0 MPa | 4350 - 13100 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Speed of Shoot, % | 35-85 |