Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific) High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled 30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | |
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Density | 1.34 - 1.40 g/cc | 0.0484 - 0.0506 lb/in³ | OSTM059 |
Solvay TOLCIDE® PS 70AF 70% tetrakis hydroxymethyl phosphonium sulfate Identification: CONCENTRATE BASED UPON TETRAKIS(HYDROXYMETHYL)PHOSPHONIUM SULPHATE (THPS) AND A BIOPENETRANTCAS: 55566-30-8Function: Concentrate for formulation into TOLCIDE® PS70A, PS50A & PS20A.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI LNP* STAT-KON* EE004 is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF/M30 HS BK 10/20% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat .. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 55/55 with low toxicity, smoke and flame evolution. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Asia Pacific) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 89/2 Flexible PVC, Insulation Insulation for special application |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
Eurostar Starflam RX06082 PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Staramide RX06082 is a Halogen Free and Red Phosphorous Free, flame Retardant, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | |
Covestro Bayblend® KU 2-1466 Polycarbonate/ABS Blend Flame retardant grade with 20% glass fiber reinforcement, high stiffness.Applications: Electrical industry.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated f.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Aclo Accutech Polycarbonate POL051G20L Glass Reinforced |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 32580B035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETThis data represents typical values for the production material. The data should not be used to write, or in p.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | Side 2, Layer 2, Silicone Property; Arlon SQA-TMS-024 |
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Density | 1.34 - 1.75 g/cc | 0.0484 - 0.0632 lb/in³ | Average value: 1.51 g/cc Grade Count:91 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |