Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.29 - 1.49 g/cc @Temperature 250 - 250 °C |
0.0466 - 0.0538 lb/in³ @Temperature 482 - 482 °F |
Average value: 1.40 g/cc Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Density | 1.37 - 1.49 g/cc | 0.0495 - 0.0538 lb/in³ | Average value: 1.43 g/cc Grade Count:3 |
Overview of materials for Polyarylsulfone (PAS), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyarylsulfone; Molded/Extruded". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.25 - 1.49 g/cc | 0.0452 - 0.0538 lb/in³ | Average value: 1.36 g/cc Grade Count:34 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 1.29 - 1.49 g/cc | 0.0466 - 0.0538 lb/in³ | Average value: 1.38 g/cc Grade Count:48 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.27 - 1.49 g/cc | 0.0459 - 0.0538 lb/in³ | Average value: 1.34 g/cc Grade Count:14 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 210/W Rigid PVC, Antishock Extrusion Various antishock profiles |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 4410 Rigid PVC, Antishock Extrusion Antishock spiral pipes |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 218/W Rigid PVC, Antishock Extrusion Lead Free Antishock profiles |
|||
Density | 1.46 - 1.49 g/cc | 0.0527 - 0.0538 lb/in³ | ASTM D792 |
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh.. |
|||
Density | 1.475 - 1.49 g/cc | 0.05329 - 0.0538 lb/in³ | ISO 1183 |
Tisan TISMOSET® Properties:Flame retardantHigh gloss surfaceImproved thermal and electircal strengthHigh impact strengthMinimized shrinkage at the presence of moldingHigh melting flow indexReduced moisture absorpti.. |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 80 Flexible PVC, Insulation General purposes |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 0179 Flexible PVC, Flame Retardant Sheathing Hydrocarbon resistant sheathing |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFX 500 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Standard sheathingInformation provided by Fainplast Compou.. |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFX 500S Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing for solar cablesInformation provided by Fainplas.. |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1183 |
Fainplast Compounds HL 90/4 Flexible PVC, Insulation for High Temperatures Operating temperature 105°C |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 70 Flexible PVC, Sheathing General purposes |
|||
Density | 1.12 - 1.49 g/cc | 0.0405 - 0.0538 lb/in³ | Average value: 1.26 g/cc Grade Count:31 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Density | 1.19 - 1.49 g/cc | 0.0430 - 0.0538 lb/in³ | Average value: 1.30 g/cc Grade Count:11 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 223F Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flexibility, good stress crack resistanceInformation provided by Fainplast Compound.. |
|||
Density | 1.08 - 1.49 g/cc | 0.0390 - 0.0538 lb/in³ | Average value: 1.13 g/cc Grade Count:26 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |