Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0621 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.25 - 1.72 g/cc
0.0452 - 0.0621 lb/in³
Average value: 1.54 g/cc Grade Count:5
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep..
Density 1.13 - 1.72 g/cc
0.0408 - 0.0621 lb/in³
Average value: 1.37 g/cc Grade Count:195
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Density 1.58 - 1.72 g/cc
0.0571 - 0.0621 lb/in³
Average value: 1.69 g/cc Grade Count:14
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Density 1.20 - 1.72 g/cc
0.0434 - 0.0621 lb/in³
Average value: 1.45 g/cc Grade Count:331
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Density 1.68 - 1.72 g/cc
0.0607 - 0.0621 lb/in³
IEC 60811
Fainplast Compounds HAX HF 108 Halogen Free PVC
Filling and bedding, designed to meet BS 6724
Density 1.68 - 1.72 g/cc
0.0607 - 0.0621 lb/in³
ISO 1183
Fainplast Compounds Hax™ HFC 0108 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 6724Information provided by Fainplast Compounds
Density 1.52 - 1.72 g/cc
0.0549 - 0.0621 lb/in³
Molded
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound
BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific ..