Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 - 76.0 MPa
7980 - 11000 psi
Average value: 64.3 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), High Impact
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Ultimate 12.4 - 76.0 MPa
1800 - 11000 psi
Average value: 26.9 MPa Grade Count:206
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Ultimate 5.50 - 76.0 MPa
798 - 11000 psi
Average value: 13.1 MPa Grade Count:17
Overview of materials for EMAAA Terpolymer
This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 48.0 - 76.0 MPa
6960 - 11000 psi
Average value: 61.4 MPa Grade Count:5
Overview of materials for Polycarbonate/Styrenic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Ultimate 32.0 - 75.8 MPa
4640 - 11000 psi
Average value: 57.6 MPa Grade Count:15
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Tensile Strength, Ultimate 21.0 - 75.8 MPa
3050 - 11000 psi
Average value: 56.7 MPa Grade Count:15
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Tensile Strength, Ultimate 25.0 - 75.5 MPa
3630 - 11000 psi
Average value: 39.2 MPa Grade Count:34
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Tensile Strength, Ultimate 11.0 - 75.8 MPa
1600 - 11000 psi
Average value: 41.7 MPa Grade Count:25
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 62.1 - 75.8 MPa
9000 - 11000 psi
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound
BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers.
Tensile Strength, Ultimate 53.0 - 76.0 MPa
7690 - 11000 psi
Average value: 61.7 MPa Grade Count:12
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..