Polymer Property : CTE, linear = 120 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 26.0 - 120 µm/m-°C
14.4 - 66.7 µin/in-°F
Average value: 85.4 µm/m-°C Grade Count:71
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
CTE, linear 100 - 120 µm/m-°C

@Temperature 20.0 °C
55.6 - 66.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
CTE, linear 108 - 120 µm/m-°C
60.0 - 66.7 µin/in-°F
Average value: 116 µm/m-°C Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
CTE, linear 120 - 120 µm/m-°C

@Temperature 100 - 200 °C
66.7 - 66.7 µin/in-°F

@Temperature 212 - 392 °F
Average value: 120 µm/m-°C Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
CTE, linear 90.0 - 120 µm/m-°C
50.0 - 66.7 µin/in-°F
ASTM D696
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide
PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon®
CTE, linear 100 - 120 µm/m-°C
55.6 - 66.7 µin/in-°F
ASTM D696
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel
PTFE G Special Compound with steelInformation provided by Guarniflon®
CTE, linear 90.0 - 120 µm/m-°C
50.0 - 66.7 µin/in-°F
ASTM D696
Guarniflon PTFE G427 Polytetrafluoroethylene 40% Bronze, 5% Molybdenum Disulfide
PTFE G Special Compound with bronze and molybdenum disulphiteInformation provided by Guarniflon®
CTE, linear 110 - 120 µm/m-°C
61.1 - 66.7 µin/in-°F
ASTM D696
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide
PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne..
CTE, linear 100 - 120 µm/m-°C
55.6 - 66.7 µin/in-°F
ASTM D696
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
CTE, linear 100 - 120 µm/m-°C

@Temperature 20.0 °C
55.6 - 66.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
CTE, linear 85.0 - 120 µm/m-°C
47.2 - 66.7 µin/in-°F
Average value: 96.4 µm/m-°C Grade Count:14
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
CTE, linear 43.2 - 120 µm/m-°C
24.0 - 66.7 µin/in-°F
Average value: 83.3 µm/m-°C Grade Count:27
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
CTE, linear 90.0 - 120 µm/m-°C
50.0 - 66.7 µin/in-°F
Average value: 98.4 µm/m-°C Grade Count:8
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
CTE, linear 31.0 - 120 µm/m-°C
17.2 - 66.7 µin/in-°F
Average value: 69.8 µm/m-°C Grade Count:10
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
CTE, linear 120 - 120 µm/m-°C

@Temperature 100 - 200 °C
66.7 - 66.7 µin/in-°F

@Temperature 212 - 392 °F
Average value: 120 µm/m-°C Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
CTE, linear 30.0 - 120 µm/m-°C
16.7 - 66.7 µin/in-°F
Average value: 68.9 µm/m-°C Grade Count:127
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..