Polymer Property : Processing Temperature = 440 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 188 - 227 °C
370 - 440 °F
Average value: 204 °C Grade Count:3
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 210 °C Grade Count:8
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 210 °C Grade Count:3
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 210 °C Grade Count:7
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 210 °C Grade Count:7
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Processing Temperature 40.0 - 227 °C
104 - 440 °F
Average value: 183 °C Grade Count:23
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Processing Temperature 204 - 227 °C
400 - 440 °F
Injection
Shuman 710H Utility Black ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Processing Temperature 204 - 227 °C
400 - 440 °F
Injection
Shuman 720H Black ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Processing Temperature 204 - 227 °C
400 - 440 °F
Injection
Shuman 730 Utility White ABS
Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc.
Processing Temperature 204 - 227 °C
400 - 440 °F
Injection
Shuman 730H White ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Processing Temperature 204 - 227 °C
400 - 440 °F
Injection
Shuman 780H Grey ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Processing Temperature 204 - 227 °C
400 - 440 °F
Shuman SP810 Black Polystyrene High Impact
Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc.
Processing Temperature 204 - 227 °C
400 - 440 °F
Shuman SP880 Grey Polystyrene High Impact
Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc.
Processing Temperature 188 - 227 °C
370 - 440 °F
Blow Molding Stock Temp.
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin
Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack..
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 211 °C Grade Count:15
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 210 °C Grade Count:5
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Processing Temperature 188 - 227 °C
370 - 440 °F
Average value: 209 °C Grade Count:8
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 210 °C Grade Count:5
Overview of materials for Polypropylene with Glass Fiber + PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va..
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 210 °C Grade Count:4
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..