Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 140 - 150 °C | 284 - 302 °F | |
PolyOne LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 120 - 150 °C | 248 - 302 °F | Average value: 138 °C Grade Count:33 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Drying Temperature | 70.0 - 150 °C | 158 - 302 °F | Average value: 98.7 °C Grade Count:15 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Drying Temperature | 130 - 150 °C | 266 - 302 °F | Average value: 148 °C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Drying Temperature | 121 - 150 °C | 250 - 302 °F | Average value: 142 °C Grade Count:30 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Drying Temperature | 50.0 - 150 °C | 122 - 302 °F | Average value: 122 °C Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton CE/60 PPS, 60% Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; .. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latiohm 80-04 PD01 G/30 PPS, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Drying Temperature | 120 - 150 °C @Time 14400 sec |
248 - 302 °F @Time 4.00 hour |
|
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 140 - 150 °C | 284 - 302 °F | Average value: 149 °C Grade Count:24 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |