Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 12.0 kV/mm | 305 kV/in | ASTM D149 |
Protective Coating PC-Crete™ Epoxy Putty PC-PUTTIES™ are hand moldable epoxy putty that are especially designed for emergency type repairs where time is of the essence.Data provided by the manufacturer. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | ASTM D149 |
Protective Coating PC-Marine™ Epoxy Putty PC-PUTTIES™ are hand moldable epoxy putty that are especially designed for emergency type repairs where time is of the essence.Data provided by the manufacturer. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | ASTM D149 |
Parker Chomerics C-Wings Heat Spreaders Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | ASTM D149 |
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | |
Permabond UV610 UV-curable Adhesive PERMABOND UV610 is a single part, fast setting, UV curable adhesive designed specifically for bonding glass and metal. Its high strength makes it suitable for a wide range of applications including .. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | |
Permabond UV670 UV-curable Adhesive PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to met.. |
|||
Dielectric Strength | 12.0 - 16.0 kV/mm | 305 - 406 kV/in | Average value: 13.7 kV/mm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 45Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 45U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-b Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Dielectric Strength | 12.0 kV/mm @Thickness 3.20 mm |
305 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 365 PC+PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | Wet, short term. ASTM D149 |
Sumitomo Bakelite North America 2008A Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | Short Time; ASTM D149 |
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | Short Time; ASTM D149 |
Plenco 08122 Polyester BMC, Compression Molded PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | |
Von Roll Isola IMI Varnish 73538 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 30°C. Usag.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | ASTM D149 |
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |
|||
Dielectric Strength | 12.0 kV/mm @Thickness 1.00 mm |
305 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Dielectric Strength | 12.0 kV/mm @Thickness 1.00 mm |
305 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Dielectric Strength | 12.0 kV/mm @Thickness 1.00 mm |
305 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Dielectric Strength | 12.0 kV/mm @Thickness 3.00 mm |
305 kV/in @Thickness 0.118 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | Insulating Strength |
China-Yixing Longly Refractories 75 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |
|||
Dielectric Strength | 12.0 - 100 kV/mm | 305 - 2540 kV/in | Average value: 25.1 kV/mm Grade Count:53 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Dielectric Strength | 12.0 kV/mm @Thickness 3.00 mm |
305 kV/in @Thickness 0.118 in |
step by step; IEC 60243 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Dielectric Strength | 12.0 kV/mm @Thickness 1.00 mm |
305 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | Short Time; ASTM D149 |
Plenco 7579 Phenolic, Granular, Compression Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |
|||
Dielectric Strength | 12.0 kV/mm @Thickness 1.60 mm |
305 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL FN215X PPE+PS Structural foam resin. 170F (77C) HDT. Improved reliability and productivity. All values at 20% weight reduction. |
|||
Dielectric Strength | 12.0 - 21.5 kV/mm @Temperature 95.0 - 150 °C |
305 - 546 kV/in @Temperature 203 - 302 °F |
Average value: 15.8 kV/mm Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Dielectric Strength | 12.0 - 21.5 kV/mm @Thickness 1.60 - 3.20 mm |
305 - 546 kV/in @Thickness 0.0630 - 0.126 in |
Average value: 15.8 kV/mm Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Dielectric Strength | 12.0 kV/mm | 305 kV/in | ST; ASTM D149 |
Sumitomo Bakelite North America FM 4004 Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004 is a fiberglass and mineral reinforced phenolic novolac compound. This compound exhibits excellent dimensional stability and good strength at elevated temperatures, and conforms to the requ.. |