Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Eraclene® MM 84 High Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® MM 84 High Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene MM 84 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 is characterized by high rigidity and good impact resistance. The resin is UV stabilized and is recommended for the production of items for outdoor exposure.Main Applications: Eraclene MM 84 is specifically designed for pails and light-weight containers. Moreover, the product is suitable to manufacture dust bins and small industrial containers.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.956 g/cc
0.956 g/cc
ISO 1183
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
14 g/10 min

@Load 5.00 kg,
Temperature 190 °C
14 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868/A
Tensile Strength at Break 20.0 MPa
2900 psi
ISO 527
Tensile Strength, Yield 28.0 MPa
4060 psi
ISO 527
Elongation at Break 550 %
550 %
ISO 527
Flexural Modulus 1.35 GPa
196 ksi
ISO 178
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ISO 180/A
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
Internal method
Vicat Softening Point 127 °C

@Load 1.00 kg
261 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746