Material Notes:
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate packed in moisture resistant cartons, Standard carton size: 25 kg palletized in 750 kg loads. Processing: Compression/Transfer/Injection. Applications: Connectors, Thermocouples, Sensors, Resistors, Potentiometers.Information provided by the Raschig Group
Physical Properties Metric English Comments
Specific Gravity 1.90 - 2.10 g/cc
1.90 - 2.10 g/cc
ISO 1183
Apparent Bulk Density 0.850 - 1.00 g/cc
0.0307 - 0.0361 lb/in³
ISO 60
Water Absorption <= 0.10 %

@Temperature 23.0 °C,
Time 86400 sec
<= 0.10 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
(longitudinal) Injection and Compression; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 - 70.0 MPa
8700 - 10200 psi
Injection and Compression; ISO 527
Modulus of Elasticity 15.0 - 18.0 GPa
2180 - 2610 ksi
Injection and Compression; ISO 527
Flexural Strength 120 - 140 MPa
17400 - 20300 psi
Injection and Compression; ISO 178
Flexural Modulus 14.0 - 16.0 GPa
2030 - 2320 ksi
Injection and Compression; ISO 178
Compressive Strength 150 - 200 MPa
21800 - 29000 psi
ISO 604
Charpy Impact Unnotched 0.800 - 1.20 J/cm²

@Temperature 23.0 °C
3.81 - 5.71 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eU
Charpy Impact, Notched 0.250 - 0.350 J/cm²

@Temperature 23.0 °C
1.19 - 1.67 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eA
Thermal Properties Metric English Comments
CTE, linear 15.0 - 20.0 µm/m-°C

@Temperature 50.0 - 150 °C
8.33 - 11.1 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Thermal Conductivity 0.600 - 0.800 W/m-K
4.16 - 5.55 BTU-in/hr-ft²-°F
ASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C
>= 392 °F
Injection; ISO 75-A
Deflection Temperature at 8.0 MPa 170 - 190 °C
338 - 374 °F
Injection; ISO 75-C
Flammability, UL94 V-0

@Thickness 5.70 mm
V-0

@Thickness 0.224 in
Shrinkage <= 0.050 %

@Temperature 110 °C,
Time 605000 sec
<= 0.050 %

@Temperature 230 °F,
Time 168 hour
Post-shrinkage; ISO 2577
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 - 1.00e+15 ohm
1.00e+14 - 1.00e+15 ohm
IEC 60093
Dielectric Constant 4.0 - 6.0

@Frequency 1.00e+6 Hz
4.0 - 6.0

@Frequency 1.00e+6 Hz
IEC 60250
5.0 - 7.0

@Frequency 100 Hz
5.0 - 7.0

@Frequency 100 Hz
IEC 60250
Dielectric Strength 0.984 - 1.38 kV/mm
25.0 - 35.0 kV/in
IEC 60243-1
15.0 - 20.0 kV/mm

@Thickness 1.00 mm
381 - 508 kV/in

@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor 0.010 - 0.030

@Frequency 100 Hz
0.010 - 0.030

@Frequency 100 Hz
IEC 60250
0.010 - 0.030

@Frequency 1.00e+6 Hz
0.010 - 0.030

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index >= 250 V
>= 250 V
CTI; IEC 60112
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 15.0 - 25.0 °C
6.00 Month

@Temperature 59.0 - 77.0 °F
Descriptive Properties Value Comments
Arc Resistance 4 Stufe
ASTM D495
Glow wire flammability test 900/1
IEC 60695 2-12
Glow wire ignitability test 900/1
IEC 60695 2-13
Water Absorption <10 mg
ISO 62; 24h / 23°C
Copyright © lookpolymers.com All Rights Reserved