SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer SCG Chemicals Co.
Trade Name EL-Pro™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electrical appliance parts, mainly for washing machine parts, e.g. base, tub, control panelInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D1505
Linear Mold Shrinkage, Flow 0.0146 cm/cm

@Thickness 2.00 mm
0.0146 in/in

@Thickness 0.0787 in
TPE Method
Linear Mold Shrinkage, Transverse 0.0112 cm/cm

@Thickness 2.00 mm
0.0112 in/in

@Thickness 0.0787 in
TPE Method
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength at Break 18.0 MPa
2610 psi
ASTM D638
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm

@Temperature -20.0 °C
0.551 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.392 J/cm

@Temperature 0.000 °C
0.735 ft-lb/in

@Temperature 32.0 °F
ASTM D256
0.588 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
ASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze 80 %

@Thickness 1.00 mm
80 %

@Thickness 0.0394 in
ASTM D1003
Gloss 30 %

@Thickness 1.00 mm
30 %

@Thickness 0.0394 in
ASTM D2457