Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Ixef®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bromine Free; Flame Retardant; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Halogen Free; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Ultra High StiffnessUses: Cell Phones; Electrical/Electronic Applications; HousingsInjection Molding Notes: Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
Dry; ISO 1183
Filler Content 50 %
50 %
Glass Fiber
Mechanical Properties Metric English Comments
Flexural Strength 240 MPa
34800 psi
ISO 178
Flexural Modulus 15.5 GPa
2250 ksi
ISO 178
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 260 °C
482 - 500 °F
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Melt Temperature 280 °C
536 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 100 °C

@Time 3600 - 10800 sec
212 °F

@Time 1.00 - 3.00 hour
Descriptive Properties Value Comments
Additive Flame Retardant
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Colors
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant