Solvay TECHNYL® 1011R PA6, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® 1011R PA6, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 6, Unfilled, lubricated, for injection molding. Available in: Asia Pacific Product Applications: TECHNYL® 1011R is used in all sectors of industry, offering an excellent flow ability. This grade is used for: Fastener, Clip, Gear, Bobbin, Hand mixer cover. This product is available in NAT color.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 1.3 %

@Temperature 23.0 °C,
Time 86400 sec
1.3 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
Linear Mold Shrinkage, Transverse 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D786
Tensile Strength, Yield 80.0 MPa
11600 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Flexural Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 2.95 GPa
428 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D265
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ASTM D648
Flammability, UL94 HB
HB
ISO 1210
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 3.40 kV/mm
86.4 kV/in
IEC 60243
Dissipation Factor 0.020
0.020
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 230 - 235 °C
446 - 455 °F
Front Barrel Temperature 245 - 250 °C
473 - 482 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 235-345°C