Material Notes:
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc

@Temperature 22.8 °C
1.14 g/cc

@Temperature 73.0 °F
ASTM D792
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
0.125inch wall
Mechanical Properties Metric English Comments
Tensile Strength, Yield 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 117 MPa
17000 psi
Max Load; ASTM D790
Flexural Modulus 5.17 GPa
750 ksi
secant; ASTM D790
6.89 GPa
1000 ksi
tangent; ASTM D790
Izod Impact, Notched 0.801 J/cm

@Temperature 22.8 °C
1.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
ASTM D648