Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0553 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.05 - 1.53 g/cc
0.0379 - 0.0553 lb/in³
Average value: 1.14 g/cc Grade Count:156
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Density 1.33 - 1.53 g/cc
0.0480 - 0.0553 lb/in³
Average value: 1.43 g/cc Grade Count:18
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Density 1.22 - 1.53 g/cc
0.0441 - 0.0553 lb/in³
Average value: 1.35 g/cc Grade Count:7
Overview of materials for Polycarbonate/Polysulfone Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o..
Density 0.940 - 1.53 g/cc
0.0340 - 0.0553 lb/in³
Average value: 1.16 g/cc Grade Count:60
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Density 1.15 - 1.53 g/cc
0.0415 - 0.0553 lb/in³
Average value: 1.29 g/cc Grade Count:98
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Density 1.11 - 1.53 g/cc
0.0401 - 0.0553 lb/in³
Average value: 1.27 g/cc Grade Count:57
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1184
Fainplast Compounds RE 410 Rigid PVC, Extrusion
Clic channels
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1184
Fainplast Compounds RK 218 Rigid PVC, Extrusion Lead Free
Rolling shutters
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1184
Fainplast Compounds RK 321 Rigid PVC, Extrusion Lead Free
Profiles
Density 1.50 - 1.53 g/cc
0.0542 - 0.0553 lb/in³
Fusor 2200
Lord Adhesives Fusor® 2200 / 2201 Urethane Adhesive
Fusor® 2200/2201 is a black equal-mix, twocomponent, paste urethane adhesive system. Fusor 2200/2201 adhesive bonds FRP, SMC, and other plastics with little surface preparation where bond strengt..
Density 1.03 - 1.53 g/cc
0.0372 - 0.0553 lb/in³
Trelleborg Offshore Vikotherm™ 73185 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Density 1.50 - 1.53 g/cc
0.0542 - 0.0553 lb/in³
Laminate
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form
Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds CL 82 Flexible PVC, Sheathing
General purposes
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds FK 93 Flexible PVC, Insulation Lead Free
General purposes
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds FKA 0753 Flexible PVC, Flame Retardant Insulation Lead Free
General purposes
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds FKA 86/1 Flexible PVC, Flame Retardant Insulation Lead Free
Power cables
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds GA 75/1 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds GA 85 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds GK 85 Flexible PVC, Flame Retardant Sheathing Lead Free
General purposes
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds GK 85/1 Flexible PVC, Flame Retardant Sheathing Lead Free
General purposes
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
IEC 60811
Fainplast Compounds HAX HF 018/25 Halogen Free PVC
Insulation; very low thickness
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
IEC 60811
Fainplast Compounds HAX HF 4022 Halogen Free PVC
General purpose
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1184
Fainplast Compounds R 218 Rigid PVC, Extrusion
Shutters and shiny profiles
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
IEC 60811
Fainplast Compounds HAX HF 4021 Halogen Free PVC
General purpose
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO 1183
Fainplast Compounds Hax™ HF 018/25 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation; very low thicknessInformation provided by Fainplast Compounds
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1184
Fainplast Compounds HG 82 Flexible PVC, Sheathing for High Temperatures
Sheathing general purposes
Density 1.44 - 1.53 g/cc
0.0520 - 0.0553 lb/in³
Molding; IS 867-1963
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App..
Density 1.09 - 1.53 g/cc
0.0394 - 0.0553 lb/in³
Average value: 1.23 g/cc Grade Count:23
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds AP 90/2 Flexible PVC, Flame Retardant Insulation
General purposes