| Category | Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone |
| Manufacturer | Aremco |
| Trade Name | Corr-Paint™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
| Solids Content | 57.4 % | 57.4 % | by weight |
| 62.1 % | 62.1 % | by volume | |
| Volatile Organic Compounds (VOC) Content | 443 g/l | 443 g/l | |
| Viscosity | 250 - 350 cP | 250 - 350 cP | |
| Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
| 44.2 microns | 1.74 mil | estimated wet film thickness | |
| Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
| 427 °C | 800 °F | Intermittent | |
| Flash Point | 46.1 °C | 115 °F |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
| 2.00 - 4.00 hour | 2.00 - 4.00 hour | Handling | |
| 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat | |
| Cure Time | >= 60.0 min | >= 1.00 hour | Air Set prior to curing |
| 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
||
| 60.0 min @Temperature 232 °C |
1.00 hour @Temperature 450 °F |
Adequate ventilation is required when curing these products. Outgassing will occur above 300°F and cease after 750°F. An additional 30 minutes is required at the highest service temperature if service temperature is below 750°F. | |
| Shelf Life | 6.00 Month | 6.00 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Green | |
| Dry Film Coverage ft2/gal | 920.3 | at 1 mil |
| Primer | Not Required | |