Material Notes:
Capron 8200CQ Blend is a medium viscosity, nylon 6 injection molding homopolymer possessing the combination of strength, stiffness and toughness properties as well as chemical and abrasion resistance. It is available in natural, heat stabilized and pigmented versions.Capron 8200CQ Blend is generally recommended for applications such as textile components, filter housings, hinges, gears, medical parts, cattle ear tags, wiring devices, plugs, receptacles, gears and connectors.Data provided by Allied Signal.Processing: Max. water content 0.25%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.Melt Temperature: 240-280 degC (464-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 10 degC (50 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO data
Water Absorption 1.6 %
1.6 %
24 hrs; ISO data
Moisture Absorption at Equilibrium 2.6 %
2.6 %
50% RH; 23°C; ISO data
Water Absorption at Saturation 9.2 %
9.2 %
in water; 23°C; ISO data
Viscosity Measurement 64
64
Formic Acid Viscosity; ISO data
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
50 mm/min; Same value from ASTM and ISO test.
Elongation at Yield 4.0 %
4.0 %
ISO Value at 50 mm/min.
4.0 %
4.0 %
ASTM Value at 50 mm/min.
Flexural Yield Strength 110 MPa
16000 psi
ASTM Data
Flexural Modulus 3.17 GPa
460 ksi
ASTM Data
Poissons Ratio 0.35
0.35
ISO data
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM and ISO test
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM Data
Processing Properties Metric English Comments
Drying Temperature 85.0 °C
185 °F