| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnite® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Arnite® TV4 261 /A PBT-GF30.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
| Water Absorption | 0.30 % | 0.30 % | Sim. To ISO 62 |
| Moisture Absorption | 0.150 % | 0.150 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 145 MPa | 21000 psi | ISO 527-1/-2 |
| Elongation at Break | 3.0 % | 3.0 % | ISO 527-1/-2 |
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| 1.10 J/cm² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | 401 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.7 @Frequency 1.00e+6 Hz |
3.7 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.9 @Frequency 100 Hz |
3.9 @Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.0025 @Frequency 100 Hz |
0.0025 @Frequency 100 Hz |
IEC 60250 |
| 0.017 @Frequency 1.00e+6 Hz |
0.017 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 400 V | 400 V | IEC 60112 |