| Category | Polymer , Thermoplastic , Nylon , Nylon 612 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 151L NC010 Nylon 612
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | |
| 1.06 g/cc | 0.0383 lb/in³ | DAM; ISO 1183 | |
| Water Absorption | 3.0 % @Thickness 2.00 mm |
3.0 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Moisture Absorption | 1.30 % @Thickness 2.00 mm |
1.30 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Viscosity Test | 95 cm³/g | 95 cm³/g | DAM; sulphuric acid 96%; ISO 307 1157 1628 |
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
| 0.011 cm/cm @Thickness 3.20 mm |
0.011 in/in @Thickness 0.126 in |
DAM | |
| Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
| 0.011 cm/cm @Thickness 3.20 mm |
0.011 in/in @Thickness 0.126 in |
DAM; ASTM D149 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 114 | 114 | DAM; ISO 2039-2 |
| Tensile Stress | 9.39 MPa @Strain 4.73 %, Temperature 150 °C |
1360 psi @Strain 4.73 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
| 10.81 MPa @Strain 0.420 %, Temperature 23.0 °C |
1568 psi @Strain 0.420 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 14.0 MPa @Strain 0.530 %, Temperature 0.000 °C |
2030 psi @Strain 0.530 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 15.75 MPa @Strain 18.94 %, Temperature 150 °C |
2284 psi @Strain 18.94 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 16.79 MPa @Strain 33.14 %, Temperature 150 °C |
2435 psi @Strain 33.14 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 17.32 MPa @Strain 47.35 %, Temperature 150 °C |
2512 psi @Strain 47.35 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 23.6 MPa @Strain 0.860 %, Temperature -40.0 °C |
3420 psi @Strain 0.860 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 38.66 MPa @Strain 1.70 %, Temperature 23.0 °C |
5607 psi @Strain 1.70 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 50.98 MPa @Strain 2.12 %, Temperature 0.000 °C |
7394 psi @Strain 2.12 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 57.27 MPa @Strain 2.97 %, Temperature 23.0 °C |
8306 psi @Strain 2.97 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 61.33 MPa @Strain 4.24 %, Temperature 23.0 °C |
8895 psi @Strain 4.24 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 71.79 MPa @Strain 3.71 %, Temperature 0.000 °C |
10410 psi @Strain 3.71 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 75.37 MPa @Strain 3.44 %, Temperature -40.0 °C |
10930 psi @Strain 3.44 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 75.89 MPa @Strain 5.30 %, Temperature 0.000 °C |
11010 psi @Strain 5.30 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 94.56 MPa @Strain 6.02 %, Temperature -40.0 °C |
13710 psi @Strain 6.02 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 97.17 MPa @Strain 8.60 %, Temperature -40.0 °C |
14090 psi @Strain 8.60 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 50%RH; ISO 527-1/-2 |
| 62.0 MPa | 8990 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 17 % | 17 % | DAM; Nominal; ISO 527-1/-2 |
| >= 50 % | >= 50 % | 50%RH; Nominal; ISO 527-1/-2 | |
| Elongation at Yield | 4.5 % | 4.5 % | DAM; ISO 527-1/-2 |
| 4.5 % | 4.5 % | DAM; ISO 527-3 | |
| 18 % | 18 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 1.70 GPa | 247 ksi | 50%RH; ISO 527-1/-2 |
| 2.40 GPa | 348 ksi | DAM; ISO 527-1/-2 | |
| 0.233 GPa @Temperature 160 °C |
33.8 ksi @Temperature 320 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 0.350 GPa @Temperature 120 °C |
50.8 ksi @Temperature 248 °F |
50%RH; ISO 11403-1 -2 | |
| 0.663 GPa @Temperature 80.0 °C |
96.2 ksi @Temperature 176 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 1.096 GPa @Temperature 40.0 °C |
159.0 ksi @Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 1.432 GPa @Temperature 30.0 °C |
207.7 ksi @Temperature 86.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 2.766 GPa @Temperature -10.0 °C |
401.2 ksi @Temperature 14.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 2.961 GPa @Temperature -40.0 °C |
429.5 ksi @Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 | |
| 3.122 GPa @Temperature -40.0 °C |
452.8 ksi @Temperature -40.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| Flexural Modulus | 1.44 GPa | 209 ksi | 50%RH; ISO 178 |
| 2.10 GPa | 305 ksi | DAM; ISO 178 | |
| Shear Modulus | 0.0946 GPa @Temperature 160 °C |
13.7 ksi @Temperature 320 °F |
DAM; Dynamic; ISO 11403-1 -2 |
| 0.1165 GPa @Temperature 120 °C |
16.90 ksi @Temperature 248 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 0.182 GPa @Temperature 70.0 °C |
26.4 ksi @Temperature 158 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 0.726 GPa @Temperature 20.0 °C |
105 ksi @Temperature 68.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 0.778 GPa @Temperature -20.0 °C |
113 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 0.828 GPa @Temperature -50.0 °C |
120 ksi @Temperature -58.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| Secant Modulus | 0.076562 GPa @Strain 36.6863 %, Temperature 100 °C |
11.105 ksi @Strain 36.6863 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
| 0.143 GPa @Strain 18.3431 %, Temperature 100 °C |
20.7 ksi @Strain 18.3431 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 | |
| 0.326 GPa @Strain 4.58579 %, Temperature 100 °C |
47.3 ksi @Strain 4.58579 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 | |
| 1.40 GPa @Strain 6.88 %, Temperature -40.0 °C |
203 ksi @Strain 6.88 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 1.75 GPa @Strain 4.24 %, Temperature 0.000 °C |
254 ksi @Strain 4.24 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 1.76 GPa @Strain 3.39 %, Temperature 23.0 °C |
255 ksi @Strain 3.39 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 2.19 GPa @Strain 3.44 %, Temperature -40.0 °C |
318 ksi @Strain 3.44 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 2.27 GPa @Strain 1.70 %, Temperature 23.0 °C |
330 ksi @Strain 1.70 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 2.40 GPa @Strain 2.12 %, Temperature 0.000 °C |
349 ksi @Strain 2.12 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 2.57 GPa @Strain 0.420 %, Temperature 23.0 °C |
373 ksi @Strain 0.420 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 2.64 GPa @Strain 0.530 %, Temperature 0.000 °C |
383 ksi @Strain 0.530 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 2.74 GPa @Strain 0.860 %, Temperature -40.0 °C |
398 ksi @Strain 0.860 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | DAM; ISO 180/1A |
| 4.50 kJ/m² | 2.14 ft-lb/in² | 50%RH; ISO 180/1A | |
| 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A | |
| 4.50 kJ/m² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
| Charpy Impact Unnotched | NB | NB | DAM; ISO 179/1eU |
| NB | NB | 50%RH; ISO 179/1eU |