| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.04 g/cc | 1.04 g/cc | DAM; ASTM D792 |
| Density | 1.04 g/cc | 0.0376 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 1.5 % @Temperature 23.0 °C |
1.5 % @Temperature 73.4 °F |
DAM; Immersion 24h; ASTM D570 |
| 2.3 % @Temperature 23.0 °C |
2.3 % @Temperature 73.4 °F |
DAM; Equilibrium 50%RH; ISO 62, Similar to | |
| 6.8 % @Temperature 23.0 °C |
6.8 % @Temperature 73.4 °F |
DAM; Saturation, immersed; ISO 62, Similar to | |
| Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.20 mm |
0.018 in/in @Thickness 0.126 in |
DAM |
| 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 | |
| Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 3.20 mm |
0.018 in/in @Thickness 0.126 in |
DAM |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 57 | 57 | 50%RH; ASTM D785 |
| Hardness, Rockwell R | 70 | 70 | 50%RH; ASTM D785 |
| Hardness, Shore D | 57 | 57 | 50%RH; ASTM D2240 |
| 70 | 70 | DAM; ASTM D2240 | |
| Tensile Strength | 41.0 MPa @Temperature 23.0 °C |
5950 psi @Temperature 73.4 °F |
50%RH; ASTM D638 |
| 48.0 MPa @Temperature 23.0 °C |
6960 psi @Temperature 73.4 °F |
DAM; ASTM D638 | |
| Tensile Strength, Yield | 31.0 MPa @Temperature 23.0 °C |
4500 psi @Temperature 73.4 °F |
DAM; ISO 527 |
| Elongation at Break | >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
50%RH; ISO 527 |
| >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
DAM; ISO 527 | |
| >= 225 % @Temperature 23.0 °C |
>= 225 % @Temperature 73.4 °F |
50%RH; ASTM D638 | |
| >= 225 % @Temperature 23.0 °C |
>= 225 % @Temperature 73.4 °F |
DAM; ASTM D638 | |
| Elongation at Yield | 29 % @Temperature 23.0 °C |
29 % @Temperature 73.4 °F |
DAM; ISO 527 |
| Tensile Modulus | 0.400 GPa @Temperature 23.0 °C |
58.0 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 0.900 GPa @Temperature 23.0 °C |
131 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 0.297 GPa @Temperature 23.0 °C |
43.1 ksi @Temperature 73.4 °F |
50%RH; ASTM D790 |
| 0.524 GPa @Temperature 23.0 °C |
76.0 ksi @Temperature 73.4 °F |
DAM; ASTM D790 | |
| Izod Impact, Unnotched | 6.93 J/cm @Temperature -40.0 °C |
13.0 ft-lb/in @Temperature -40.0 °F |
DAM; ASTM D256 |
| 8.00 J/cm @Temperature -20.0 °C |
15.0 ft-lb/in @Temperature -4.00 °F |
DAM; ASTM D256 | |
| 11.7 J/cm @Temperature 0.000 °C |
21.9 ft-lb/in @Temperature 32.0 °F |
DAM; ASTM D256 | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DAM; ASTM D256 | |
| Charpy Impact Unnotched | NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DAM; ISO 179/1eU | |
| Charpy Impact, Notched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
| 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 7.10 J/cm² @Temperature 23.0 °C |
33.8 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA | |
| 12.9 J/cm² @Temperature 23.0 °C |
61.4 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA | |
| Tensile Impact Strength | 1310 kJ/m² @Temperature 23.0 °C |
623 ft-lb/in² @Temperature 73.4 °F |
DAM; Long specimen; ASTM D1822 |
| 1363 kJ/m² @Temperature 23.0 °C |
648.6 ft-lb/in² @Temperature 73.4 °F |
50%RH; Long specimen; ASTM D1822 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM D696 |
| 200 µm/m-°C @Temperature 23.0 - 55.0 °C |
111 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 | |
| 200 µm/m-°C @Temperature 23.0 - 55.0 °C |
111 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| CTE, linear, Transverse to Flow | 180 µm/m-°C @Temperature 23.0 - 55.0 °C |
100 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
| 180 µm/m-°C @Temperature 23.0 - 55.0 °C |
100 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| Melting Point | 216 °C | 421 °F | DAM; ASTM D3418 |
| 218 °C | 424 °F | DAM; 10°C/min; ISO 11357-1/-3 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | DAM; ISO 75-1/-2 |
| 170 °C | 338 °F | DAM; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 47.0 °C | 117 °F | DAM; ISO 75-1/-2 |
| 52.0 °C | 126 °F | DAM; ASTM D648 | |
| UL RTI, Electrical | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
DAM; UL 746B |
| 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
DAM; UL 746B | |
| UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
DAM; UL 746B |
| 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
DAM; UL 746B | |
| UL RTI, Mechanical without Impact | 95.0 °C @Thickness 0.750 mm |
203 °F @Thickness 0.0295 in |
DAM; UL 746B |
| 100 °C @Thickness 1.50 mm |
212 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
DAM; UL 746B | |
| Flammability, UL94 | HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
DAM; IEC 60695-11-10 |
| HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
DAM; UL94 | |
| HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 | |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
DAM; IEC 60695-11-10 | |
| HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; UL94 | |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
DAM; UL94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | >= 600 V @Temperature 23.0 °C |
>= 600 V @Temperature 73.4 °F |
DAM; UL 746A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 °C | 464 °F | DAM; optimum; Extrusion |
| 235 - 250 °C | 455 - 482 °F | DAM; Extrusion | |
| 260 - 280 °C | 500 - 536 °F | DAM; Injection Molding | |
| 270 °C | 518 °F | DAM; optimum; Injection Molding | |
| Mold Temperature | 70.0 °C | 158 °F | DAM; Optimum; Injection Molding |