| Category | Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 30% Glass Fiber Filled |
| Manufacturer | EMS-Grivory (EMS-CHEMIE) |
| Trade Name | Grivory® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | EMS-Grivory Grivory® LV-3A H PA12-GF30.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
| Water Absorption | 1.4 % | 1.4 % | ISO 62 |
| Moisture Absorption | 0.600 % | 0.600 % | ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 | 80 | conditioned, 15s; ISO 868 |
| Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
| Tensile Strength at Break | 110 MPa | 16000 psi | conditioned; ISO 527-1/-2 |
| 120 MPa | 17400 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 6.0 % | 6.0 % | dry; ISO 527-1/-2 |
| 6.0 % | 6.0 % | conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 5.70 GPa | 827 ksi | conditioned; ISO 527-1/-2 |
| 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
| 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
| Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | conditioned; ISO 179/1eA |
| 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 180 °C | 356 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 165 °C | 329 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 90.0 °C | 194 °F | ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
| Comparative Tracking Index | 575 V | 575 V | conditioned; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive | Cooling and climate control | |
| Fuel systems | ||
| Form | Granules | |
| Industry & Consumer goods | Heating systems | |
| Processing | Injection Molding | |
| Product Attributes | Hydrolysis resistant | |
| Special Characteristics | High impact or impact modified | |
| Improved heat resistance | ||
| Improved UV resistance (outdoor use) |