| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled |
| Manufacturer | EPICHEM srl |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | ASTM D792, ISO 1183 |
| Water Absorption | 6.5 % @Temperature 23.0 °C |
6.5 % @Temperature 73.4 °F |
24h; ASTM D570, ISO 62 |
| Linear Mold Shrinkage | 0.0030 - 0.012 cm/cm | 0.0030 - 0.012 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell L | 115 | 115 | ASTM D785, ISO 2039/2 |
| Tensile Strength, Yield | 160 MPa | 23200 psi | ASTM D638, ISO R527 |
| Elongation at Break | 4.0 % | 4.0 % | ASTM D638, ISO R527 |
| Flexural Strength | 220 MPa | 31900 psi | ASTM D790, ISO 178 |
| Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790, ISO 178 |
| Izod Impact, Notched | 0.500 - 0.700 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.937 - 1.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 105 °C | 221 °F | 20000 h; VDE 0304/P2-1, IEC 216 |
| 110 °C | 230 °F | 5000 h; VDE 0304/P2-1, IEC 216 | |
| 180 °C | 356 °F | few hours; VDE 0304/P2-1, IEC 216 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 185 °C | 365 °F | ASTM D648, ISO 75 |
| Vicat Softening Point | 205 °C @Load 5.00 kg |
401 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
| 210 °C @Load 0.999 kg |
410 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A | |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
|
| HB @Thickness 3.20 mm |
HB @Thickness 0.126 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257, IEC 93 |
| Dielectric Constant | 3.4 @Frequency 1000 Hz |
3.4 @Frequency 1000 Hz |
ASTM D150, IEC 250 |
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149, IEC 243 |
| Dissipation Factor | 0.013 @Frequency 1000 Hz |
0.013 @Frequency 1000 Hz |
ASTM D150, IEC 250 |
| Comparative Tracking Index | 550 V | 550 V | VDE 0303-P1, IEC 112 |