| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.41 g/cc | 0.0509 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.200 % <br>@Temperature 23.0 °C |
0.200 % <br>@Temperature 73.4 °F |
50% RH; ISO 960 |
| Linear Mold Shrinkage, Flow | 0.0050 cm/cm | 0.0050 in/in | Eurotec |
| Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 105 MPa | 15200 psi | ISO 527 |
| Elongation at Break | 3.0 % | 3.0 % | ISO 527 |
| Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 6.00 kJ/m² <br>@Temperature -30.0 °C |
2.86 ft-lb/in² <br>@Temperature -22.0 °F |
ISO 180/1A |
| 7.00 kJ/m² <br>@Temperature 23.0 °C |
3.33 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 45.0 kJ/m² <br>@Temperature -30.0 °C |
21.4 ft-lb/in² <br>@Temperature -22.0 °F |
ISO 180/1U |
| 50.0 kJ/m² <br>@Temperature 23.0 °C |
23.8 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 225 °C | 437 °F | [10 K/min], ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75 |
| Vicat Softening Point | 205 °C <br>@Load 5.10 kg |
401 °F <br>@Load 11.2 lb |
ISO 306 |
| Flammability, UL94 | HB <br>@Thickness 0.750 mm |
HB <br>@Thickness 0.0295 in |
|
| HB <br>@Thickness 1.60 mm |
HB <br>@Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
| Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
| Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
| Drying Temperature | 120 °C | 248 °F | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
| Moisture Content | <= 0.080 % | <= 0.080 % | ISO 960 |
| Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Fast |