| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Glass Fiber Filler |
| Manufacturer | Eurotec |
| Trade Name | Tecolen® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eurotec® Tecolen® CP10 GR50 NL PPCP, 50% glass fiber reinforced, natural.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 90.0 MPa | 13100 psi | ISO 527 |
| Elongation at Break | 3.0 % | 3.0 % | ISO 527 |
| Tensile Modulus | 11.0 GPa | 1600 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
| 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
| Deflection Temperature at 1.8 MPa (264 psi) | 145 °C | 293 °F | ISO 75 |
| Flammability, UL94 | HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
|
| HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 200 - 240 °C | 392 - 464 °F | |
| Feed Temperature | <= 60.0 °C | <= 140 °F | Throat |
| Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
| Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Medium - Fast |