| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant |
| Manufacturer | Eurotec |
| Trade Name | Tecolen® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eurotec® Tecolen® CP30 NL XC30 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 20.0 MPa | 2900 psi | ISO 527 |
| Elongation at Break | >= 100 % | >= 100 % | ISO 527 |
| Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
| 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
| Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75 |
| Flammability, UL94 | V-2 @Thickness 0.750 mm |
V-2 @Thickness 0.0295 in |
|
| V-2 @Thickness 1.60 mm |
V-2 @Thickness 0.0630 in |
||
| Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
| 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI; IEC 60695 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 200 - 240 °C | 392 - 464 °F | |
| Feed Temperature | <= 60.0 °C | <= 140 °F | Throat |
| Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
| Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Medium - Fast |