ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Plexus
Trade Name Plexus™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive , high toughness.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Viscosity 50000 - 70000 cP
50000 - 70000 cP
B
100000 - 125000 cP
100000 - 125000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.6 - 20.7 MPa
2700 - 3000 psi
Elongation at Break 100 - 125 %
100 - 125 %
Shear Strength 12.1 - 15.5 MPa
1750 - 2250 psi
Processing Properties Metric English Comments
Pot Life 4.0 - 6.0 min
4.0 - 6.0 min
Descriptive Properties Value Comments
Color Blue, black, or yellow
Fixture Time 15-18 minutes
Mix Ratio 10:1
By volume