Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos ABS Lustran® QE 1455/L2, Injection Grade  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® QE 1455/L2, Injection Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection molding grade, increased heat resistance, medium gloss, UV-stabilized grade.Applications: Automotive: body parts.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Melt Flow 10 g/10 min

@Load 10.0 kg,
Temperature 220 °C
10 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7110 psi
Elongation at Yield 2.0 %
2.0 %
Tensile Modulus 2.60 GPa
377 ksi
Charpy Impact Unnotched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
Vicat Softening Point 102 °C
216 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Strength 29.0 kV/mm
737 kV/in
Comparative Tracking Index 600 V
600 V