| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Impact Modified |
| Manufacturer | Kolon |
| Trade Name | Kocetal® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Kolon KOCETAL® EL304 Toughened Grade Acetal Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
| Moisture Absorption at Equilibrium | 0.25 % | 0.25 % | 60% RH; ASTM D570 |
| Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
| Melt Flow | 9.0 g/10 min | 9.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 76 | 76 | ASTM D785 |
| Tensile Strength | 43.0 MPa | 6240 psi | ASTM D638 |
| Elongation at Break | 85 % | 85 % | ASTM D638 |
| Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
| Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
| Melting Point | 166 °C | 331 °F | ASTM D1525 |
| Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 82.0 °C | 180 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 3.7 | 3.7 | ASTM D150 |
| Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
| Dissipation Factor | 0.0060 @Frequency 1.00e+6 Hz |
0.0060 @Frequency 1.00e+6 Hz |
ASTM D150 |