| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant |
| Manufacturer | LG Chemical |
| Trade Name | LUPOL |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical LUPOL GP1007F Flame Retardant PP.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.010 | 0.010 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 29.4 MPa @Thickness 3.20 mm |
4270 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | 100 % @Thickness 3.20 mm |
100 % @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 36.3 MPa @Thickness 6.40 mm |
5260 psi @Thickness 0.252 in |
10mm/min; ASTM D790 |
| Flexural Modulus | 1.57 GPa @Thickness 6.40 mm |
228 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
| Izod Impact, Notched | 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 120 °C @Thickness 3.20 mm |
248 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
| UL RTI, Electrical | 120 °C @Thickness >=0.750 mm |
248 °F @Thickness >=0.0295 in |
|
| 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 120 °C @Thickness >=0.750 mm |
248 °F @Thickness >=0.0295 in |
|
| 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 120 °C @Thickness >=0.750 mm |
248 °F @Thickness >=0.0295 in |
|
| 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| Flammability, UL94 | V-0 @Thickness >=0.750 mm |
V-0 @Thickness >=0.0295 in |
|
| V-0 @Thickness >=1.50 mm |
V-0 @Thickness >=0.0591 in |
||
| V-0 @Thickness >=3.00 mm |
V-0 @Thickness >=0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
| Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
| 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
||
| 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
||
| High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
|
| >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
||
| >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
| Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
| Front Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
| Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
| Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Injection Molding |
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
| Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm | Injection Molding |