ND Industries 530 Shaft & Bearing Retainer Retaining Compound

Category Polymer , Adhesive , Thermoset
Manufacturer ND Industries, Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ND Industries 530 Shaft & Bearing Retainer Retaining Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General DescriptionA high strength adhesive for retention of cylindrical components, where disassembly is not required.Typical Usesrotors, shafts, bushings, bearings, and pulleysMeets military spec MIL-R-46082 Type I
Physical Properties Metric English Comments
Viscosity 100 - 500 cP
100 - 500 cP
Mechanical Properties Metric English Comments
Shear Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
With Primer (Fixture)
10.0 - 20.0 min
0.167 - 0.333 hour
On steel (Fixture)
1440 min
24.0 hour
On Steel (Full)
1440 min
24.0 hour
With Primer (Full)
Descriptive Properties Value Comments
Color Green
Gap Fill, in. 0.005