| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 - 1.24 g/cc | 0.0405 - 0.0448 lb/in³ | Average value: 1.17 g/cc Grade Count:32 |
| Moisture Absorption at Equilibrium | 1.50 - 3.90 % | 1.50 - 3.90 % | Average value: 2.29 % Grade Count:7 |
| Water Absorption at Saturation | 5.00 - 8.50 % | 5.00 - 8.50 % | Average value: 7.00 % Grade Count:7 |
| Moisture Vapor Transmission | 0.360 - 3.10 cc-mm/m²-24hr-atm | 0.914 - 7.87 cc-mil/100 in²-24hr-atm | Average value: 1.13 cc-mm/m²-24hr-atm Grade Count:26 |
| Water Vapor Transmission | 14.3 - 217 g/m²/day | 0.920 - 14.0 g/100 in²/day | Average value: 126 g/m²/day Grade Count:3 |
| 275 - 275 g/m²/day @Temperature 40.0 - 40.0 °C |
17.7 - 17.7 g/100 in²/day @Temperature 104 - 104 °F |
Average value: 275 g/m²/day Grade Count:1 | |
| Oxygen Transmission | 0.00400 - 0.600 cc-mm/m²-24hr-atm | 0.0102 - 1.52 cc-mil/100 in²-24hr-atm | Average value: 0.0397 cc-mm/m²-24hr-atm Grade Count:28 |
| Oxygen Transmission Rate | 0.310 - 1.55 cc/m²/day | 0.0200 - 0.0998 cc/100 in²/day | Average value: 1.08 cc/m²/day Grade Count:4 |
| Viscosity | 1.09 - 4.57 cP @Temperature 190 - 230 °C |
1.09 - 4.57 cP @Temperature 374 - 446 °F |
Average value: 1.29e+6 cP Grade Count:1 |
| 170000 - 1.40e+7 cP @Temperature 200 - 230 °C |
170000 - 1.40e+7 cP @Temperature 392 - 446 °F |
Average value: 1.29e+6 cP Grade Count:11 | |
| 170000 - 1.40e+7 cP @Shear Rate 60.0 - 270 1/s |
170000 - 1.40e+7 cP @Shear Rate 60.0 - 270 1/s |
Average value: 1.29e+6 cP Grade Count:11 | |
| Thickness | 15.2 - 63.5 microns | 0.600 - 2.50 mil | Average value: 32.0 microns Grade Count:6 |
| Melt Flow | 0.800 - 22.0 g/10 min | 0.800 - 22.0 g/10 min | Average value: 5.88 g/10 min Grade Count:27 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 84.0 - 104 | 84.0 - 104 | Average value: 93.2 Grade Count:13 |
| Tensile Strength, Ultimate | 37.0 - 74.0 MPa | 5370 - 10700 psi | Average value: 58.8 MPa Grade Count:4 |
| Tensile Strength, Yield | 43.0 - 94.0 MPa | 6240 - 13600 psi | Average value: 67.3 MPa Grade Count:13 |
| Film Elongation at Break, MD | 70.0 - 390 % | 70.0 - 390 % | Average value: 238 % Grade Count:16 |
| Film Elongation at Break, TD | 85.0 - 390 % | 85.0 - 390 % | Average value: 237 % Grade Count:7 |
| Elongation at Break | 130 - 330 % | 130 - 330 % | Average value: 220 % Grade Count:4 |
| Elongation at Yield | 1.00 - 8.00 % | 1.00 - 8.00 % | Average value: 5.20 % Grade Count:8 |
| Modulus of Elasticity | 1.08 - 3.65 GPa | 156 - 529 ksi | Average value: 2.26 GPa Grade Count:14 |
| Flexural Yield Strength | 108 - 150 MPa | 15700 - 21800 psi | Average value: 128 MPa Grade Count:5 |
| Flexural Modulus | 3.10 - 4.70 GPa | 450 - 682 ksi | Average value: 4.12 GPa Grade Count:5 |
| Secant Modulus, MD | 1.02 - 3.50 GPa | 148 - 508 ksi | Average value: 1.91 GPa Grade Count:5 |
| Secant Modulus, TD | 1.00 - 3.50 GPa | 145 - 508 ksi | Average value: 1.86 GPa Grade Count:5 |
| Izod Impact, Notched | 0.304 - 0.900 J/cm | 0.570 - 1.69 ft-lb/in | Average value: 0.583 J/cm Grade Count:7 |
| Coefficient of Friction | 0.200 - 0.500 | 0.200 - 0.500 | Average value: 0.365 Grade Count:3 |
| Tear Strength Test | 500 - 1300 | 500 - 1300 | Average value: 690 Grade Count:4 |
| Elmendorf Tear Strength MD | 260 - 460 g | 260 - 460 g | Average value: 367 g Grade Count:3 |
| Elmendorf Tear Strength TD | 300 - 440 g | 300 - 440 g | Average value: 357 g Grade Count:3 |
| Elmendorf Tear Strength, MD | 2.02 - 30.2 g/micron | 51.3 - 767 g/mil | Average value: 14.3 g/micron Grade Count:6 |
| Elmendorf Tear Strength, TD | 0.525 - 28.9 g/micron | 13.3 - 733 g/mil | Average value: 14.1 g/micron Grade Count:6 |
| Taber Abrasion, mg/1000 Cycles | 1.20 - 2.20 | 1.20 - 2.20 | Average value: 1.65 Grade Count:4 |
| Film Tensile Strength at Break, MD | 37.0 - 317 MPa | 5370 - 46000 psi | Average value: 96.7 MPa Grade Count:16 |
| Film Tensile Strength at Break, TD | 44.0 - 195 MPa | 6380 - 28300 psi | Average value: 102 MPa Grade Count:7 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 40.0 - 130 µm/m-°C | 22.2 - 72.2 µin/in-°F | Average value: 87.5 µm/m-°C Grade Count:15 |
| 110 - 130 µm/m-°C @Temperature 100 - 100 °C |
61.1 - 72.2 µin/in-°F @Temperature 212 - 212 °F |
Average value: 120 µm/m-°C Grade Count:3 | |
| Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | Average value: 2.40 J/g-°C Grade Count:15 |
| Thermal Conductivity | 0.340 - 0.360 W/m-K | 2.36 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.341 W/m-K Grade Count:15 |
| Melting Point | 156 - 195 °C | 313 - 383 °F | Average value: 176 °C Grade Count:31 |
| Crystallization Temperature | 144 - 163 °C | 291 - 325 °F | Average value: 156 °C Grade Count:13 |
| Deflection Temperature at 0.46 MPa (66 psi) | 80.0 - 100 °C | 176 - 212 °F | Average value: 92.0 °C Grade Count:12 |
| Vicat Softening Point | 155 - 174 °C | 311 - 345 °F | Average value: 165 °C Grade Count:12 |
| Glass Transition Temp, Tg | 48.0 - 73.9 °C | 118 - 165 °F | Average value: 61.3 °C Grade Count:24 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.51 - 1.54 | 1.51 - 1.54 | Average value: 1.53 Grade Count:14 |
| Haze | 0.500 - 7.00 % | 0.500 - 7.00 % | Average value: 1.88 % Grade Count:21 |
| Gloss | 70.0 - 100 % | 70.0 - 100 % | Average value: 86.9 % Grade Count:18 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 4.70e+12 - 1.20e+13 ohm-cm | 4.70e+12 - 1.20e+13 ohm-cm | Average value: 8.35e+12 ohm-cm Grade Count:6 |
| Surface Resistance | 1.90e+15 - 2.70e+15 ohm | 1.90e+15 - 2.70e+15 ohm | Average value: 2.10e+15 ohm Grade Count:7 |
| Dielectric Constant | 4.80 - 5.60 | 4.80 - 5.60 | Average value: 5.30 Grade Count:15 |
| Dissipation Factor | 0.180 - 0.220 | 0.180 - 0.220 | Average value: 0.213 Grade Count:15 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Average value: 208 °C Grade Count:8 |
| Melt Temperature | 240 - 250 °C | 464 - 482 °F | Average value: 243 °C Grade Count:10 |