| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ B65 G30 black IG Polyamide 6 (Nylon 6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.36 g/cc | 0.0491 lb/in³ | ±0.03 g/cm³; DIN 53479 |
| Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 235 °C |
10 g/10 min @Load 4.76 lb, Temperature 455 °F |
ISO 1133 |
| Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 235 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 455 °F |
cm³/10min; ISO 1133 |
| Ash | 30 % | 30 % | ISO 3451 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 150 MPa @Temperature 23.0 °C |
21800 psi @Temperature 73.4 °F |
ISO 527-2/5 |
| Elongation at Break | 3.0 % @Temperature 23.0 °C |
3.0 % @Temperature 73.4 °F |
ISO 527-2/5 |
| Tensile Modulus | 8.30 GPa @Temperature 23.0 °C |
1200 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | ISO 3146 |
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous (GTP 50% Tensile); IEC 60216 |
| 190 °C | 374 °F | Short Time; IEC 60216 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | Unannealed; ISO 75-2/A |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 93 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 93 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Filler / Reinforcement | Glass Fiber Reinforcement, 30% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Regional Availability | Europe | |
| RoHS Compliance | RoHS Compliant |