| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.36 g/cc | 0.0491 lb/in³ | ±0.03 g/cm³; DIN 53479 |
| Ash | >= 20 % | >= 20 % | ISO 3451 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 91.0 MPa @Temperature 23.0 °C |
13200 psi @Temperature 73.4 °F |
ISO 527-2/5 |
| Elongation at Break | 2.5 % @Temperature 23.0 °C |
2.5 % @Temperature 73.4 °F |
ISO 527-2/5 |
| Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | 3.10 J/cm² @Temperature -30.0 °C |
14.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 0.320 J/cm² @Temperature -30.0 °C |
1.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | ISO 3146 |
| Maximum Service Temperature, Air | 95.0 °C | 203 °F | Continuous (GTP 50% Tensile); IEC 60216 |
| 190 °C | 374 °F | Short Time; IEC 60216 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | Unannealed; ISO 75-2/B |
| Flammability, UL94 | V-2 @Thickness 0.800 mm |
V-2 @Thickness 0.0315 in |
ALL; Internal Method |
| Glow Wire Test | 960 °C @Thickness 0.800 - 1.60 mm |
1760 °F @Thickness 0.0315 - 0.0630 in |
Ignition Temperature; IEC 60695-2-13 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
| Comparative Tracking Index | 400 V | 400 V | Solution A; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Flame Retardant | |
| Halogen Free | ||
| Laser Markable | ||
| Low (to None) Phosphorus Content | ||
| Filler / Reinforcement | GlassMineral, 20% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Regional Availability | Europe | |