| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Nylatron® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.21 g/cc | 0.0437 lb/in³ | ISO 1183-1 |
| Moisture Absorption at Equilibrium | 2.5 % | 2.5 % | 50% RH |
| Water Absorption at Saturation | 6.9 % | 6.9 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 85 | 85 | ISO 2039-2 |
| Ball Indentation Hardness | 170 MPa | 24700 psi | ISO 2039-1 |
| Tensile Strength | 87.0 MPa | 12600 psi | at Yield; ISO 527-1/-2 |
| Elongation at Break | 25 % | 25 % | ISO 527-1/-2 |
| Elongation at Yield | 4.0 % | 4.0 % | ISO 527-1/-2 |
| Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527-1/-2 |
| Compressive Strength | 35.0 MPa @Strain 1 % |
5080 psi @Strain 1 % |
ISO 604 |
| 67.0 MPa @Strain 2 % |
9720 psi @Strain 2 % |
ISO 604 | |
| 92.0 MPa @Strain 5 % |
13300 psi @Strain 5 % |
ISO 604 | |
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1/1eU |
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179-1/1eA |
| Coefficient of Friction, Dynamic | 0.40 - 0.60 | 0.40 - 0.60 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 100 µm/m-°C @Temperature 23.0 - 100 °C |
55.6 µin/in-°F @Temperature 73.4 - 212 °F |
|
| Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
| Melting Point | 220 °C | 428 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
| Maximum Service Temperature, Air | 70.0 °C | 158 °F | Continuous; 20,000 h |
| 85.0 °C | 185 °F | Continuous; 5,000 h | |
| Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C | 185 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | |
| Oxygen Index | 25 % | 25 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.0e+12 ohm-cm | >= 1.0e+12 ohm-cm | IEC 60093 |
| Surface Resistivity per Square | >= 1.0e+11 ohm | >= 1.0e+11 ohm | IEC 60093 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| European Food 1935/2004 | Yes | Yes | |
| FDA | Yes | Yes | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Unacceptable | Unacceptable | |
| Acids, Weak | Limited | Limited | |
| Alcohols | Limited | Limited | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Limited | Limited | |
| Chlorinated Solvents | Limited | Limited | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |