Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
DAM; ASTM D792
Water Absorption 0.60 %
0.60 %
24 hrs, DAM; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
0.125 in, DAM; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88
88
ASTM D785
Tensile Strength at Break 152 MPa
22000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
0.0591 in, BK
HB
HB
0.118 in, BK
Processing Properties Metric English Comments
Melt Temperature 282 - 304 °C
540 - 580 °F
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.20 %
0.20 %
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Screw Speed 40 - 120 rpm
40 - 120 rpm
Users viewing this material also viewed the following: