| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Cycoloy® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
| Tensile Strength, Yield | 44.0 MPa | 6380 psi | 50 mm/min; ISO 527 |
| 45.0 MPa | 6530 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 90 % | 90 % | Type I, 50 mm/min; ASTM D638 |
| 100 % | 100 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 4.0 % | 4.0 % | 50 mm/min; ISO 527 |
| Tensile Modulus | 2.17 GPa | 315 ksi | 50 mm/min; ASTM D638 |
| Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
| 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.00 GPa | 290 ksi | 2 mm/min; ISO 178 |
| 2.02 GPa | 293 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
| 5.30 J/cm @Temperature -30.0 °C |
9.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 47.0 kJ/m² | 22.4 ft-lb/in² | 80*10*4; ISO 180/1A |
| 41.0 kJ/m² @Temperature -30.0 °C |
19.5 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 4.40 J/cm² @Temperature -30.0 °C |
20.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 45.0 J @Temperature 23.0 °C |
33.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| 45.0 J @Temperature -30.0 °C |
33.2 ft-lb @Temperature -22.0 °F |
ASTM D3763 | |
| 47.0 J @Temperature -40.0 °C |
34.7 ft-lb @Temperature -40.0 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 120 °C | 248 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 98.0 °C @Thickness 3.20 mm |
208 °F @Thickness 0.126 in |
unannealed; ASTM D648 |