| Category | Polymer , Thermoplastic , ABS Polymer |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP FARADEX |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
| 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 | |
| Moisture Absorption | 0.200 % | 0.200 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
| 0.0030 cm/cm @Time 86400 sec |
0.0030 in/in @Time 24.0 hour |
ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
| 0.0040 cm/cm @Time 86400 sec |
0.0040 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 37.0 MPa | 5370 psi | ISO 527 |
| 39.0 MPa | 5660 psi | ASTM D638 | |
| Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
| 42.0 MPa | 6090 psi | ASTM D638 | |
| Elongation at Break | 2.8 % | 2.8 % | ISO 527 |
| 6.2 % | 6.2 % | ASTM D638 | |
| Elongation at Yield | 2.2 % | 2.2 % | ISO 527 |
| 2.6 % | 2.6 % | ASTM D638 | |
| Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
| 3.15 GPa | 457 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
| 75.0 MPa | 10900 psi | ASTM D790 | |
| Flexural Modulus | 2.80 GPa | 406 ksi | ISO 178 |
| 3.04 GPa | 441 ksi | ASTM D790 | |
| Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 3.07 J/cm | 5.75 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 88.0 °C @Thickness 3.20 mm |
190 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | ASTM D257 |
| Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
| Shielding Effectiveness | 50 - 65 dB @Thickness 3.00 mm |
50 - 65 dB @Thickness 0.118 in |
SABIC Method |