| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL PX9406P PPE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Melt Index of Compound | 10 g/10 min <br>@Load 5.00 kg,<br> Temperature 280 °C |
10 g/10 min <br>@Load 11.0 lb,<br> Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
| 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 76.0 MPa | 11000 psi | Type I, 50 mm/min; ASTM D638 |
| 76.0 MPa | 11000 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 9.4 % | 9.4 % | 50 mm/min; ISO 527 |
| 9.7 % | 9.7 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 4.7 % | 4.7 % | Type I, 50 mm/min; ASTM D638 |
| 4.7 % | 4.7 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.73 GPa | 396 ksi | 1 mm/min; ISO 527 |
| 2.80 GPa | 406 ksi | 50 mm/min; ASTM D638 | |
| Flexural Yield Strength | 113 MPa | 16400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 114 MPa | 16500 psi | 2 mm/min; ISO 178 | |
| 114 MPa | 16500 psi | 6.4 mm; ASTM D790 | |
| Flexural Modulus | 2.58 GPa | 374 ksi | 2 mm/min; ISO 178 |
| 2.84 GPa | 412 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| 2.84 GPa | 412 ksi | 6.4 mm; ASTM D790 | |
| Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
| 0.600 J/cm <br>@Temperature -30.0 °C |
1.12 ft-lb/in <br>@Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1A |
| 8.00 kJ/m² <br>@Temperature -30.0 °C |
3.81 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 0.800 J/cm² <br>@Temperature -30.0 °C |
3.81 ft-lb/in² <br>@Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 52.0 J <br>@Temperature 23.0 °C |
38.4 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 244 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 118 °C <br>@Thickness 3.20 mm |
244 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| 122 °C <br>@Thickness 6.40 mm |
252 °F <br>@Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
| 150 °C | 302 °F | Rate A/120; ISO 306 | |
| UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
| UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
| UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
| Flammability, UL94 | V-0 <br>@Thickness 0.750 mm |
V-0 <br>@Thickness 0.0295 in |
UL 94 by SABIC-IP |
| 5VB <br>@Thickness 2.00 mm |
5VB <br>@Thickness 0.0787 in |
UL 94 by SABIC-IP | |
| 5VA <br>@Thickness 2.50 mm |
5VA <br>@Thickness 0.0984 in |
UL 94 by SABIC-IP | |
| Glow Wire Test | 750 °C | 1380 °F | IEC 60695-2-13 |
| 775 °C | 1430 °F | IEC 60695-2-13 | |
| 960 °C <br>@Thickness 0.750 mm |
1760 °F <br>@Thickness 0.0295 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |