| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Noryl EN212 PPE+PS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D 792 |
| Water Absorption | 0.070 % @Time 86400 sec |
0.070 % @Time 24.0 hour |
ASTM D 570 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 115 | 115 | ASTM D 785 |
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 50 mm/min; ASTM D 638 |
| Elongation at Break | 45 % | 45 % | Type I, 50 mm/min; ASTM D 638 |
| Flexural Yield Strength | 78.0 MPa | 11300 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
| Flexural Modulus | 2.51 GPa | 364 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
| Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.49 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
| 2.93 J/cm @Temperature 23.0 °C |
5.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 | |
| Gardner Impact | 6.00 J @Temperature -40.0 °C |
4.43 ft-lb @Temperature -40.0 °F |
ASTM D 3029 |
| 25.0 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
ASTM D 3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 110 °C @Thickness 6.40 mm |
230 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 98.0 °C @Thickness 6.40 mm |
208 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
| UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
| UL RTI, Mechanical without Impact | 95.0 °C | 203 °F | UL 746B |
| Flammability, UL94 | V-1 @Thickness 1.49 mm |
V-1 @Thickness 0.0587 in |
UL 94 |
| V-0 @Thickness 5.99 mm |
V-0 @Thickness 0.236 in |
UL 94 | |
| Oxygen Index | 29.6 % | 29.6 % | LOI; ASTM D 2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 2.65 @Frequency 50.0 - 60.0 Hz |
2.65 @Frequency 50.0 - 60.0 Hz |
ASTM D 150 |
| Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in oil; ASTM D 149 |
| Dissipation Factor | 0.00070 @Frequency 50.0 - 60.0 Hz |
0.00070 @Frequency 50.0 - 60.0 Hz |
ASTM D 150 |
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten, PLC code 7; ASTM D 495 |
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V | PLC code 1; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | PLC code 4; UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Radiant Panel Listing | YES | UL Tested |
| UV-light, water exposure/immersion | F1 | UL 746C |